BE Opaline Striker

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
Barbara Elmore
Posts: 19
Joined: Wed Nov 19, 2003 5:47 pm
Location: State Road NC

BE Opaline Striker

Post by Barbara Elmore »

Tried to put opaline striker over BE turquoise and it has turned brown. Have not read anything that suggested it was reactive........Any suggestions?
Thanks, Barbara Hale Elmore

"Good judgement comes from experience. Experience comes from bad judgement" Indian Proverb
Morganica
Posts: 1079
Joined: Mon May 19, 2003 6:19 pm
Location: Portland, OR
Contact:

Re: BE Opaline Striker

Post by Morganica »

Pics, please? Are we talking frit, sheet..?

It's not supposed to contain copper-reactive stuff (sulfur/selenium/lead)...so are you sure it's opaline striker? Could it possibly be reactive cloud opal or translucent white? Both of those look sorta like opaline in the raw state and they definitely will react...
Cynthia Morgan
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com

"I wrote, therefore I was." (me)
Barbara Elmore
Posts: 19
Joined: Wed Nov 19, 2003 5:47 pm
Location: State Road NC

Re: BE Opaline Striker

Post by Barbara Elmore »

Sheet. Definitely opaline striker. The only thing I can think of is maybe my kiln temp is off from the 1490 suggested top temp. I am refining one piece as a test tonight.
Thanks, Barbara Hale Elmore

"Good judgement comes from experience. Experience comes from bad judgement" Indian Proverb
Barbara Elmore
Posts: 19
Joined: Wed Nov 19, 2003 5:47 pm
Location: State Road NC

Re: BE Opaline Striker

Post by Barbara Elmore »

Test piece came out from second firing (in a different kiln) just the same as first, dark, dark chocolate brown over the turquoise opal. Stumped.
Thanks, Barbara Hale Elmore

"Good judgement comes from experience. Experience comes from bad judgement" Indian Proverb
Warren Weiss
Posts: 137
Joined: Thu Mar 13, 2003 8:06 pm
Location: Richmond, VA

Re: BE Opaline Striker

Post by Warren Weiss »

Barbara,

Ask Bullseye on their website.

Warren
Barbara Elmore
Posts: 19
Joined: Wed Nov 19, 2003 5:47 pm
Location: State Road NC

Re: BE Opaline Striker

Post by Barbara Elmore »

Thanks, Warren, I posted it on their site and will contact Amy Ferber when she returns to portland.
Thanks, Barbara Hale Elmore

"Good judgement comes from experience. Experience comes from bad judgement" Indian Proverb
Morganica
Posts: 1079
Joined: Mon May 19, 2003 6:19 pm
Location: Portland, OR
Contact:

Re: BE Opaline Striker

Post by Morganica »

Hmmm. If you have a piece left over, try firing it on its own, without the turquoise. This one's really got me going.
Cynthia Morgan
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com

"I wrote, therefore I was." (me)
Barbara Elmore
Posts: 19
Joined: Wed Nov 19, 2003 5:47 pm
Location: State Road NC

Re: BE Opaline Striker

Post by Barbara Elmore »

OK!
Thanks, Barbara Hale Elmore

"Good judgement comes from experience. Experience comes from bad judgement" Indian Proverb
Post Reply