I've been using Wissmach 90 for the last year or so and perhaps have an insight others might find of interest. Or this might just be a 'well duh!' comment. The published information about their irids is that irid initially fired down is brilliant color, fired up is reduced color, and capped disappears. What I have found in firing irid down and refiring is that the color remains virtually unchanged when refired irid up and the color still disappears if capped. My process temp was 1485F (higher than I normally fire) and the irid was a little rough to the touch.
Jerry

Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: No registered users and 12 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com