Devit on Wissmach 90 and 96

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
Barbara Elmore
Posts: 19
Joined: Wed Nov 19, 2003 5:47 pm
Location: State Road NC

Devit on Wissmach 90 and 96

Post by Barbara Elmore »

Anyone else having problems with the newer COE's of Wissmach fusible? I fired 2 layers 96, full fuse, then slumped them and the white on top of the black devited horribly at 1175. Clean going in, mold sprayed with MR97, nothing unusual. Haven't seen devit that bad at that temp ever!
Thanks, Barbara Hale Elmore