source for mica flakes

Postby mikefromitaly » Fri Feb 20, 2015 6:00 pm

Hello friends+

i am looking for gold,silver and coloured mica flaxed in different size.

I foound this in India but in big quantity by wholesalers.

Any dealer source where to get less quantity?
any help will be appreciated

thank you

mike
thanks for sharing !

mike from italy


"secret of success?... passion & experience"

[url] http://www.picturetrail.com/mikefromitaly [/url]

rosanna gusler
Posts: 730
Joined: Mon Mar 10, 2003 2:22 pm
Location: wanchese north carolina
Contact:

Re: source for mica flakes

Postby rosanna gusler » Fri Feb 20, 2015 7:07 pm

artist, owner of wanchese art studio, marine finisher

Bert Weiss
Posts: 2338
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Re: source for mica flakes

Postby Bert Weiss » Fri Feb 20, 2015 7:21 pm

Brad sells Sepp Leaf micas'
http://www.warmglass.org/othersupplies
Bert

Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions

Brad Walker
Site Admin
Posts: 1362
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: source for mica flakes

Postby Brad Walker » Fri Feb 20, 2015 9:29 pm

Bert Weiss wrote:Brad sells Sepp Leaf micas'
http://www.warmglass.org/othersupplies


Thanks for the plug, Bert. We do sell them, but only the powder, not the flake. I don't believe they sell the flake, but if they do I could get them.

By the way, Sepp Leaf are by far the best micas I've tried. Fire to 1650F, use with sifter, brush, or airbrush.

Bert Weiss
Posts: 2338
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Re: source for mica flakes

Postby Bert Weiss » Sat Feb 21, 2015 12:56 pm

Brad Walker wrote:
Bert Weiss wrote:Brad sells Sepp Leaf micas'
http://www.warmglass.org/othersupplies


Thanks for the plug, Bert. We do sell them, but only the powder, not the flake. I don't believe they sell the flake, but if they do I could get them.

By the way, Sepp Leaf are by far the best micas I've tried. Fire to 1650F, use with sifter, brush, or airbrush.
Having tried many micas myself, my favorite is a white one called Super Sprarkle. It is a relatively large particle. I believe the micas from Sepp are manufactured now by BASF. The company has changed hands a few times over the past decade. There are also Chinese knockoffs.
Bert



Bert Weiss Art Glass*

http://www.customartglass.com

Furniture Lighting Sculpture Tableware

Architectural Commissions

Brad Walker
Site Admin
Posts: 1362
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: source for mica flakes

Postby Brad Walker » Sat Feb 21, 2015 3:01 pm

Bert Weiss wrote:... my favorite is a white one called Super Sparkle...


That might be our best selling one. I'm not sure if it's the mica or the name.

Bert Weiss
Posts: 2338
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Re: source for mica flakes

Postby Bert Weiss » Sat Feb 21, 2015 3:23 pm

Brad Walker wrote:
Bert Weiss wrote:... my favorite is a white one called Super Sparkle...


That might be our best selling one. I'm not sure if it's the mica or the name.
With the metallic colors, they don't really match up to real metals. The golds are brown, and the silvers gray. The whites do stay white though. I often mix the Super Sparkle with mother of pearl, which is a finely ground white.

I can mix some micas in with my Sunshine colors and fire (to 1420ºF) color side down, on the tin side of float glass, in a stainless steel slump mold, and get a bowl in a single firing. The interior is glass with color behind it. The exterior is matte finished color. You can't do that with fusing glasses because they will melt in to a pile in the bottom of the mold. Float holds up. I do have to put a fresh coat of kilnwash on the mold, on after a hot firing.
Bert



Bert Weiss Art Glass*

http://www.customartglass.com

Furniture Lighting Sculpture Tableware

Architectural Commissions

mikefromitaly
Posts: 67
Joined: Thu Apr 03, 2003 7:47 am
Location: italy-sicily
Contact:

Re: source for mica flakes

Postby mikefromitaly » Sat Feb 21, 2015 3:30 pm

thank you for ypur reply


I need no Mica Powder but flakes in different size..
So Sepp Leaf has as well ?

thank you

mike


Image
thanks for sharing !

mike from italy


"secret of success?... passion & experience"

[url] http://www.picturetrail.com/mikefromitaly [/url]

nbobb
Posts: 25
Joined: Mon Aug 16, 2004 1:35 pm
Location: California
Contact:

Re: source for mica flakes

Postby nbobb » Mon May 18, 2015 6:03 pm

There's a company called K2 that used to sell mica in two particle sizes. Their "sparkle" was the powder and their "glitter" was larger particles. Nobody carries these any more, so I contacted the company and they wanted me to import at least a kilogram of each color. The guy said he was cutting me some slack, as companies usually bought in 25 kilogram quantities. That was a little more than I needed, so I didn't do it. I do have some on hand that I bought from my last source but someday that will be gone.

Every once in a while, I begin a new quest and continue the hunt for larger particles. I've tried the cosmetic sources but the FDA limits cosmetic mica to 150 microns, which I'm assuming is pretty fine (I don't have anything to measure a micron with). I've found you also have to be careful about their mica flakes and glitter because they're not always real mica and might even be a form of plastic.

My next attempt was mica for industrial applications but I got confused real fast there because there are so many different kinds and uses.

Mike, I hope you find some mica flakes and, if you do, maybe you'll let me know.
Nancy Bobb
Firewalker Studio
http://www.firewalkerstudio.com

Bert Weiss
Posts: 2338
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Re: source for mica flakes

Postby Bert Weiss » Tue May 19, 2015 12:30 pm

mikefromitaly wrote:thank you for ypur reply


I need no Mica Powder but flakes in different size..
So Sepp Leaf has as well ?

thank you

mike


Image

Those pictures look like mica flakes. That is completely different. The micas I refer to have been industrially processed in to small particles and treated to have colors.
Bert



Bert Weiss Art Glass*

http://www.customartglass.com

Furniture Lighting Sculpture Tableware

Architectural Commissions

Valerie Adams
Posts: 587
Joined: Mon Apr 19, 2004 2:49 pm
Location: Santa Rosa, California
Contact:

Re: source for mica flakes

Postby Valerie Adams » Tue May 19, 2015 7:33 pm

I've bought them from vendors on Etsy and Ebay. Don't know this vendor but did a quick Google of Mica Flakes:
http://usartquest.com/proddetail.php?prod=PFX701_master

Michael Stevens
Posts: 71
Joined: Thu Dec 26, 2019 2:52 pm

Re: source for mica flakes

Postby Michael Stevens » Sat Jan 18, 2020 7:53 pm

I can easily find mica flakes, but after reading what Bert was saying, they need to. be treated? these commercial products look nice that he sells. is it really better to buy the products or is it easy enough to get good results diy

Michael Stevens
Posts: 71
Joined: Thu Dec 26, 2019 2:52 pm

Re: source for mica flakes

Postby Michael Stevens » Fri Jan 24, 2020 10:06 am

does anyone know if colored micah powders used in. make up can be used in fusing?

Brad Walker
Site Admin
Posts: 1362
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: source for mica flakes

Postby Brad Walker » Sat Jan 25, 2020 9:14 am

Michael Stevens wrote:does anyone know if colored micah powders used in. make up can be used in fusing?


Most likely the color will change or fade, but it's worth a try.

Ed Cantarella
Posts: 155
Joined: Mon Feb 26, 2018 3:49 pm
Location: Highland, Michigan, USA

Re: source for mica flakes

Postby Ed Cantarella » Mon Jan 27, 2020 3:45 pm

I've been using mica powder from an ebayer "contrysoapfolk". Golds, silvers and pink hold up good. Purple and green both became silvery-grey schmutz - very unattractive unless that's what you want.
HER last words were, "I'm melting, melting . . . " Dissenting opinions generally welcome for comic relief or personal edification. Sometimes both.


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: No registered users and 38 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com

cron