RE-slumping - WarmGlass.com

RE-slumping

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Tony Smith, Brad Walker

Post Reply
Aglassygirl303
Posts: 47
Joined: Sun Nov 08, 2009 10:08 pm

RE-slumping

Postby Aglassygirl303 » Sat Mar 14, 2015 1:43 pm

Hello all, I just peeked into my kiln at a beautiful 14" bowl and noticed that one of the edges has a scalloped raised edge. The kiln is at 600 and coming down. It already annealed for two hours. I'm not going to like this ripple. Can I just start now and go ahead and run it through the slumping schedule again or do I have to wait until it is 100 degrees and fuse flat again and re slump? My instincts are saying to just re slump now...

Brad Walker
Site Admin
Posts: 1356
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: RE-slumping

Postby Brad Walker » Sat Mar 14, 2015 2:41 pm

You can just start now and re-slump.


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: No registered users and 52 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com