angle grinder without water supply?

Postby SandyS » Mon May 25, 2015 10:08 pm

Hi,
I'm looking to get an angle grinder but I don't have a water supply in my studio. Is it possible to use one without water? I think I've heard of using oil? Or is it possible to rig up a water supply with a bucket hung high?

Thanks
Sandy

Brad Walker
Site Admin
Posts: 1372
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: angle grinder without water supply?

Postby Brad Walker » Mon May 25, 2015 10:42 pm

Look for PVA grinding discs. Made for marble, but will work on glass.

Tony Smith
Posts: 1037
Joined: Sun Mar 09, 2003 5:59 pm
Location: Massachusetts, USA
Contact:

Re: angle grinder without water supply?

Postby Tony Smith » Tue May 26, 2015 5:07 am

A lot of people use them inside large, plastic storage tubs to contain the spray. Then you only need enough water to cover the glass.

Tony
The tightrope between being strange and being creative is too narrow to walk without occasionally landing on both sides..." Scott Berkun

Bert Weiss
Posts: 2338
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Re: angle grinder without water supply?

Postby Bert Weiss » Tue May 26, 2015 10:32 am

I was lucky to find a backpack sprayer on sale, cheap. This works fine for my wet grinder and my wet saw. I wear the water on my back and give it a pump or 2 every now and then.
Bert

Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions

charlie
Posts: 961
Joined: Mon Mar 10, 2003 3:08 pm

Re: angle grinder without water supply?

Postby charlie » Thu May 28, 2015 10:39 pm

it's not much water. i used to use a 2 gallon jug with a hole and tap in the side up high on a shelf above my wbs for this. most of the stuff you can get at home depot in the garden sprinkler aisle: drip system stuff.

SandyS
Posts: 6
Joined: Sun Feb 19, 2012 12:28 am

Re: angle grinder without water supply?

Postby SandyS » Sat May 30, 2015 6:46 pm

thanks everyone! any suggestions on which grinder to buy or what features to look for?

Sandy

Dick
Posts: 80
Joined: Sun May 01, 2005 9:34 pm
Location: San Diego
Contact:

Re: angle grinder without water supply?

Postby Dick » Sat Jun 13, 2015 7:13 pm

If you are buying a grinder anyway and have the money, buy a wet grinder now, and you will have it for when you do get a water source. I like the Alpha but Bob has stuff to look at on His Glassworks, so check them out.


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: Google [Bot] and 63 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com