PVA Dry Disc Polishing

Postby Linda Gilpin » Sun Jun 07, 2015 8:40 pm

Hello - I saw a comment on this and now can't seem to find it. Is it possible to use PVA Diamond Grinding Discs (using them dry not wet) and get a good fire polish? Are the discs used with a polishing machine or a grinder? Any recommendations on brands or grit (and suppliers) would be much appreciated! Would it be better to just get a wet belt sander if I wouldn't have the need for it very often?

Sorry, I'm not a tool girl!

Barry Kaiser
Posts: 287
Joined: Mon Jul 25, 2005 6:54 pm
Location: North Carolina
Contact:

Re: PVA Dry Disc Polishing

Postby Barry Kaiser » Mon Jun 08, 2015 9:13 am

Having never tried dry diamond sanding, I will venture an answer.
The reason we use water is to cool the diamond. They tend to heat up rapidly. In heating up they would destroy the bond holding them to the surface, thus freeing themselves and no longer being effective.
Don't think it would work for long, but maybe someone who has had success would chime in here.

Barry

charlie
Posts: 961
Joined: Mon Mar 10, 2003 3:08 pm

Re: PVA Dry Disc Polishing

Postby charlie » Tue Jun 09, 2015 11:18 pm

they do countertop edging in the field with diamond pads on grinders without water all the time. they may be bonded differently, or the diamonds are in the hard rubber and aren't dislodged with use.

Marty
Posts: 853
Joined: Mon Mar 10, 2003 3:58 pm
Location: Maine
Contact:

Re: PVA Dry Disc Polishing

Postby Marty » Wed Jun 10, 2015 10:26 pm

Or the stone is much less susceptible to cracking from the heat generated by the dry process.

charlie
Posts: 961
Joined: Mon Mar 10, 2003 3:08 pm

Re: PVA Dry Disc Polishing

Postby charlie » Wed Jun 10, 2015 10:40 pm

[quote="Marty"]Or the stone is much less susceptible to cracking from the heat generated by the dry process.[/quote]

i was referring to the bonding agent in the pad not breaking down and releasing the diamonds.

Marty
Posts: 853
Joined: Mon Mar 10, 2003 3:58 pm
Location: Maine
Contact:

Re: PVA Dry Disc Polishing

Postby Marty » Thu Jun 11, 2015 5:02 pm

Charlie- That may be but the main reason for not running those things dry is the thermal affect on the glass. The stone guys are muy macho- no stinkin' water and no stinkin' dust masks and no stinkin' ear or eye protection either.

Bert Weiss
Posts: 2338
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Re: PVA Dry Disc Polishing

Postby Bert Weiss » Fri Jun 12, 2015 9:32 pm

Glass guys dry grind all the time, with carbide sanding belts. I dry grind with my inch and an eighth by twenty one belt sander. The belts are specifically designed for dry grinding glass. If you build up too much heat, little chips fly off. I don't know anything about dry grinding with diamonds. I have a wet grinder for that.
Bert

Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions

Dick
Posts: 80
Joined: Sun May 01, 2005 9:34 pm
Location: San Diego
Contact:

Re: PVA Dry Disc Polishing

Postby Dick » Sat Jun 13, 2015 6:46 pm

Always better to add even a little water. I have used the peel off pads from CR Laurence that they use for windshields etc. and I suppose if you went super slow it might work, but faster, and more efficient and healthy if you use water. Even when cutting kiln shelves, which can be done dry, it is faster, easier and more healthy to add water


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: No registered users and 57 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com