Hi all,

I am going to have a go at fusing some coarse frit in Kaiser board molds to create pattern bars. My bars will end up 10cm x 4cm x 4cm. Is there a way I can calculate the fusing schedule for these size pieces as I will be firing 12 of them and don't want to mess it up. I have never done anything thicker than a 6mm platter.

I have looked at the Bullseye site but can't find an answer for this particular size. Is there a brilliant table like the potmelt one that calculates it once you enter the sizes.

Many thanks
Tracey
Charlotte Kay
Posts: 15
Joined: Sat Dec 12, 2009 10:43 pm
Location: Northern California

Re: Bullseye schedules

Post by Charlotte Kay »

Have you seen this Bullseye tip sheet for thick slabs?
https://www.bullseyeglass.com/images/st ... _slabs.pdf