Getting cerium oxide out of small bubbles.

Postby Andy G. » Fri Aug 28, 2015 11:38 pm

Hi. I recently bought a flat lap wheel and while I LOVE it, I'm a bit frustrated how to get the dried bits of cerium oxide out of some of the small bubbles after the polishing step. Is it just a matter of wetting the piece and then digging them out with a toothpick?

Any hints or tips would be greatly appreciated.

Thank you, warm glass community!

-Andy

Brad Walker
Site Admin
Posts: 1372
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Getting cerium oxide out of small bubbles.

Postby Brad Walker » Sat Aug 29, 2015 8:41 am


charlie
Posts: 961
Joined: Mon Mar 10, 2003 3:08 pm

Re: Getting cerium oxide out of small bubbles.

Postby charlie » Sat Aug 29, 2015 11:01 am

car wash water jet

Andy G.
Posts: 11
Joined: Mon Jul 24, 2006 2:34 pm
Location: Burbank, California
Contact:

Re: Getting cerium oxide out of small bubbles.

Postby Andy G. » Sat Aug 29, 2015 11:53 am

Love the soap idea. WIll definitely try it.

Thanks so much.

Bert Weiss
Posts: 2338
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Re: Getting cerium oxide out of small bubbles.

Postby Bert Weiss » Sat Aug 29, 2015 3:41 pm

The pressure washer at the carwash is the least expensive tool rental out there. You put a few quarters in the machine, and you have a pressure washer in your hand. Bring some foam, to cushion your glass, and shoot away. They even give you the soap.
Bert

Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions

Valerie Adams
Posts: 587
Joined: Mon Apr 19, 2004 2:49 pm
Location: Santa Rosa, California
Contact:

Re: Getting cerium oxide out of small bubbles.

Postby Valerie Adams » Sat Aug 29, 2015 10:33 pm

Buy an old Water Pik at a thrift store. Mini water jet!


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: No registered users and 49 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com