Borax or boric acid?

Postby Terry Gallentine » Mon Aug 31, 2015 2:03 pm

Which is a stronger flux, borax or boric acid? Are there any other notable differences in the way they work between the two?

Bert Weiss
Posts: 2338
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Re: Borax or boric acid?

Postby Bert Weiss » Mon Aug 31, 2015 2:28 pm

All I know is that 20 mule team borax works. I never tried anything else. Some will crystalize at the bottom of the bottle, just pour the liquid off and it works. This stuff is cheap.
Bert

Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions

charlie
Posts: 961
Joined: Mon Mar 10, 2003 3:08 pm

Re: Borax or boric acid?

Postby charlie » Mon Aug 31, 2015 9:23 pm

borax: Na2B4O7

boric acid: H3BO3

they are not interchangeable and not the same.


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: No registered users and 50 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com