Postby rosanna gusler » Thu Oct 22, 2015 11:34 am

hi there . i have a bowl with thompsons liquid bright gold fired on and i want to take it off. i can not remember if sulphuric or nitric is the acid of chouce. help? rosanna
artist, owner of wanchese art studio, marine finisher

Kevin Midgley
Posts: 713
Joined: Mon Mar 10, 2003 11:36 am
Location: Tofino, British Columbia, Canada

Re: remove fired liquid bright gold

Postby Kevin Midgley » Thu Oct 22, 2015 3:37 pm

BonAmi cleaner will remove it.

Brad Walker
Site Admin
Posts: 1362
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: remove fired liquid bright gold

Postby Brad Walker » Thu Oct 22, 2015 3:41 pm

Nitric acid, usually as aqua regia (which is a nitric and hydrochloric mixture), but nitric alone will do it. I don't think sulfuric acid will dissolve gold unless it's really concentrated.

I suspect sandblasting would work, too.

Bert Weiss
Posts: 2338
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Re: remove fired liquid bright gold

Postby Bert Weiss » Fri Oct 23, 2015 12:23 am

In the stained glass world, black patina is nitric acid. All I know is that this dissolves vitreous enamels. I would guess it works on gold.
Bert

Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: No registered users and 27 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com