architectural glass mounting ... rubber/epoxy? - WarmGlass.com

architectural glass mounting ... rubber/epoxy?

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Tony Smith, Brad Walker

Post Reply
tonyroberts
Posts: 23
Joined: Thu Dec 16, 2004 5:59 pm
Location: Liverpool UK
Contact:

architectural glass mounting ... rubber/epoxy?

Postby tonyroberts » Fri Nov 20, 2015 9:31 am

Hi all... good to see you all still here!

I wish to mount thick cast glass - like dalles, but glass cast and stained in my kilns, 15-25mm thick - in a resilient framework, able to withstand occasional vibration. The Liverpool Metropolitan Cathedral has its acres of glass set in a sort of black rubbery matrix, which would be perfect! But - what is it? It looks rather like the rubbery stuff that they lay down under the play equipment in children's playgrounds.

DonMcClennen
Posts: 364
Joined: Sun Mar 09, 2003 9:09 pm
Location: Ontario

Re: architectural glass mounting ... rubber/epoxy?

Postby DonMcClennen » Fri Nov 20, 2015 11:58 am

I'm thinking it might be a form of a material like Thiokol which is black and is/was used to install car windshields... flexible and very strong..
"The Glassman"

tonyroberts
Posts: 23
Joined: Thu Dec 16, 2004 5:59 pm
Location: Liverpool UK
Contact:

Re: architectural glass mounting ... rubber/epoxy?

Postby tonyroberts » Fri Nov 20, 2015 3:25 pm

Thanks.... but no, this stuff is two-three inches deep, more like the dimensions of the concrete in modern architectural stained glass panels.

??? Tony

Marty
Posts: 851
Joined: Mon Mar 10, 2003 3:58 pm
Location: Maine
Contact:

Re: architectural glass mounting ... rubber/epoxy?

Postby Marty » Fri Nov 20, 2015 6:48 pm


Bert Weiss
Posts: 2337
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Re: architectural glass mounting ... rubber/epoxy?

Postby Bert Weiss » Sat Nov 21, 2015 11:44 am

You can get silicone epoxy that comes in 2 parts. Some are clear and others not.

I am a fan of using L screws. They are minimally visible, and will not let the load fall off.
Bert

Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions

Valerie Adams
Posts: 587
Joined: Mon Apr 19, 2004 2:49 pm
Location: Santa Rosa, California
Contact:

Re: architectural glass mounting ... rubber/epoxy?

Postby Valerie Adams » Sat Nov 21, 2015 12:23 pm

You can get black flexible grout but that's assuming the glass is mounted to something I believe.


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: No registered users and 24 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com