Hi Guys,
I have a 1" thick rigidized fiber board shelf that I've been using off & on for a few years. I just had an opal piece stick to it and tear some pretty good-sized chunks out of the surface. Anyone have suggestions about how to patch & level the surface? I have some liquid rigidizer & a couple corner chunks of the same board that I had cut off to make the board fit my oval kiln. Do you think I'd have any luck trying to grind up the board & make a patching paste with the liquid rigidizer? Is there anything else that might work? Thanks!

Valerie Adams
Posts: 587
Joined: Mon Apr 19, 2004 2:49 pm
Location: Santa Rosa, California
Contact:

Re: Patching a fiber board shelf

Postby Valerie Adams » Thu Dec 10, 2015 5:53 pm

Can you simply flip it and use the other side?

If not, JenKen kilns sells a patch compound for their fiber kilns, which I've used before. I'd contact Mike and ask about it.

Bert Weiss
Posts: 2338
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Re: Patching a fiber board shelf

Postby Bert Weiss » Fri Dec 11, 2015 1:04 pm

Yes, grind up some scrap board, mix with rigidizer and spackle the board. If you have already used colloidal silica rigidizer, go ahead and use that. The boards are originally made with colloidal alumina rigidizer. This is less sticky to the glass being fired.
Bert

Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions

Steph Mader
Posts: 58
Joined: Tue Mar 11, 2003 1:45 am
Location: Freeland, WA
Contact:

Re: Patching a fiber board shelf

Postby Steph Mader » Fri Dec 11, 2015 4:19 pm

Thanks for the info. The board was pretty rough on both sides when I got it & I rigidized it myself at the time. I used it for a long time with 1/8" fiber paper & dry kiln wash dusted on, but that won't work with what I'm doing now. So I'll try the grind & patch and see how it goes. I appreciate the advice!

charlie
Posts: 961
Joined: Mon Mar 10, 2003 3:08 pm

Re: Patching a fiber board shelf

Postby charlie » Fri Dec 18, 2015 10:28 pm

i used the cement pad of my driveway for a large flat grinding surface.

Steph Mader
Posts: 58
Joined: Tue Mar 11, 2003 1:45 am
Location: Freeland, WA
Contact:

Re: Patching a fiber board shelf

Postby Steph Mader » Sun Jan 24, 2016 12:09 am

That's so funny. If it EVER dries out here in Washington, I might try that! Also, hubby used to fair the hulls on great big racing sailboats, I'll bet he has some tricks.


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: No registered users and 42 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com