Leatherbarrow's Crackle Book is Available

Postby Lynn Perry » Wed Dec 23, 2015 4:14 pm

I bought Bob's book from his website yesterday. It is in pdf form and about $18 US. It is a very well-done book both in content and organization and a bargain. He has plans to publish at least two more.
Lynn Perry

JestersBaubles
Posts: 691
Joined: Fri Feb 25, 2011 12:01 am
Location: North Logan, UT
Contact:

Re: Leatherbarrow's Crackle Book is Available

Postby JestersBaubles » Wed Dec 23, 2015 4:39 pm

I started reading it last night. VERY well written and great information.

Having taken a couple of classes with Bob, the information is just like what is taught in his classes. Definitely a bargain.

Dana W.

Barbel
Posts: 17
Joined: Sat Dec 10, 2011 11:09 pm
Location: Ocean- Newport, North Carolina

Re: Leatherbarrow's Crackle Book is Available

Postby Barbel » Wed Dec 23, 2015 5:16 pm

Great book,
Wonderful classes,
Terrific guy!
I really enjoy reading and listening to sound technical instruction and advice. What an inspiration!
Barbel

Maggie Abdel Rahman
Posts: 36
Joined: Tue Nov 06, 2007 10:16 am

Re: Leatherbarrow's Crackle Book is Available

Postby Maggie Abdel Rahman » Mon Jan 18, 2016 8:54 pm

Thanks the information which came right in time. I have been thinking how to produce this effect and the book gives very valuable instructions.

Emily Will
Posts: 27
Joined: Fri Dec 14, 2012 1:08 am

Re: Leatherbarrow's Crackle Book is Available

Postby Emily Will » Mon Jan 18, 2016 9:30 pm

I purchased the book when it was first mentioned, read it, and followed the directions to produce a halfway decent first attempt. It is well work the $18. I'm going to Brad's class on special effects (including crackle) at the end of the month and will be a little bit ahead of the game:)

Emily

Emily Will
Fused Glass Artist
http://IntenseGlass.com
919-556-7414

glass-lady
Posts: 18
Joined: Sun Apr 25, 2004 2:43 pm
Location: Wilmington, NC
Contact:

Re: Leatherbarrow's Crackle Book is Available

Postby glass-lady » Thu Feb 04, 2016 12:55 pm

I bought this book and it is excellent. On the long list of projects to work.


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: No registered users and 42 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com

cron