Bullseye & Uroboros air pollution problems

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
Mark Wright
Posts: 49
Joined: Mon Dec 13, 2010 12:43 pm
Location: Raleigh, NC

Bullseye & Uroboros air pollution problems

Post by Mark Wright »

I ran across this news article on Facebook dated Feb. 14, 2016:
"Bullseye Glass, Southeast Portland’s globally renowned supplier of art and architectural glass, altered its production processes this week in response to concerns about the factory’s effect on local air quality.
Bullseye has passed Oregon Department of Environmental Quality tests twice in the past year but, nonetheless, last Wednesday The Portland Mercury broke the news that the state DEQ believed Bullseye was behind high levels of arsenic and cadmium in the air in Southeast Portland.
“We understand the concerns and take public health and the environment seriously,” Bullseye Glass responded in a press release. “That is why, upon being contacted by DEQ last week, we made a voluntary decision to suspend the use of cadmium and arsenic in our glass-making process.”

Link:
http://www.opb.org/artsandlife/article/ ... emissions/
Brad Walker
Site Admin
Posts: 1540
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Bullseye & Uroboros air pollution problems

Post by Brad Walker »

Already a thread on this: http://www.warmglass.com/phpBB3/viewtop ... =8&t=42369

And several related topics in the Business Forum.
Terry Gallentine
Posts: 195
Joined: Mon Jul 19, 2004 2:08 pm
Location: River Falls, WI
Contact:

Re: Bullseye & Uroboros air pollution problems

Post by Terry Gallentine »

This is hearsay, but what I heard was that Bullseye was quite a bit behind schedule in regard to air quality testing. This plus them maintaining their manufacturing facility in a residential area and not changing their formulations to minimize the amounts of cadmium and arsenic are going to present problems for them.
Marty
Posts: 862
Joined: Mon Mar 10, 2003 3:58 pm
Location: Maine
Contact:

Re: Bullseye & Uroboros air pollution problems

Post by Marty »

...and for us.
Morganica
Posts: 1079
Joined: Mon May 19, 2003 6:19 pm
Location: Portland, OR
Contact:

Re: Bullseye & Uroboros air pollution problems

Post by Morganica »

Terry Gallentine wrote:This is hearsay, but what I heard was that Bullseye was quite a bit behind schedule in regard to air quality testing. This plus them maintaining their manufacturing facility in a residential area and not changing their formulations to minimize the amounts of cadmium and arsenic are going to present problems for them.
Yes, it is hearsay.
Cynthia Morgan
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com

"I wrote, therefore I was." (me)
Post Reply