Postby smallbitz » Thu Mar 24, 2016 10:03 am

What is the best way to hold/secure a drop bowl while grinding and polishing the rim flat on a lap? I'm afraid it's going to fly out of my hands. I've put so much work into it I really don't want to end up plastering it on the wall. Sure would appreciate some suggestions.

The Hobbyist
Posts: 303
Joined: Sun Mar 09, 2003 7:09 pm
Location: Sun City West (NW Phoenix), AZ
Contact:

Re: Drop Vessel on Flat Lap

Postby The Hobbyist » Thu Mar 24, 2016 11:21 am

I think I'm not the only one that tapes handles on the backside. The most difficult part is finding duct tape that won't loose its bond when wet. HIS Glassworks carries some that I use and recommend. I'll take and post pictures today.

Jim "The Hobbyist"
"With or without religion, good people can behave well and bad people can do evil; but for good people to do evil—that takes religion. " Steven Weinberg

Marty
Posts: 853
Joined: Mon Mar 10, 2003 3:58 pm
Location: Maine
Contact:

Re: Drop Vessel on Flat Lap

Postby Marty » Thu Mar 24, 2016 12:36 pm

I've changed over to gorilla tape for handles, no failures so far.

smallbitz
Posts: 154
Joined: Sat Jun 27, 2009 8:44 am
Location: Florida

Re: Drop Vessel on Flat Lap

Postby smallbitz » Thu Mar 24, 2016 12:47 pm

Thanks so much! I would really appreciate pics if you get a chance.

The Hobbyist
Posts: 303
Joined: Sun Mar 09, 2003 7:09 pm
Location: Sun City West (NW Phoenix), AZ
Contact:

Re: Drop Vessel on Flat Lap

Postby The Hobbyist » Thu Mar 24, 2016 3:11 pm

Put one on each side.

handle.jpg
"With or without religion, good people can behave well and bad people can do evil; but for good people to do evil—that takes religion. " Steven Weinberg

smallbitz
Posts: 154
Joined: Sat Jun 27, 2009 8:44 am
Location: Florida

Re: Drop Vessel on Flat Lap

Postby smallbitz » Thu Mar 24, 2016 3:44 pm

Perfect! Many thanks!


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: Google [Bot] and 72 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com