Best Glue for Garden Stakes - WarmGlass.com

Best Glue for Garden Stakes

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Tony Smith, Brad Walker

Post Reply
grammy
Posts: 26
Joined: Fri Nov 17, 2006 10:07 am
Location: Charlotte NC
Contact:

Best Glue for Garden Stakes

Postby grammy » Fri Mar 25, 2016 10:45 am

I am replacing some glass for a client in their garden stakes. So these will be outside. The stakes do not have a way to "clip" in the glass, only glueing to the metal. What glue would be best? E6000?

Dick
Posts: 80
Joined: Sun May 01, 2005 9:34 pm
Location: San Diego
Contact:

Re: Best Glue for Garden Stakes

Postby Dick » Fri Mar 25, 2016 3:26 pm

I don't trust e6000 as I have had some failures. Loctite h30cl hysol works great and stays crystal clear.

grammy
Posts: 26
Joined: Fri Nov 17, 2006 10:07 am
Location: Charlotte NC
Contact:

Re: Best Glue for Garden Stakes

Postby grammy » Fri Mar 25, 2016 9:43 pm

Thank you.

DonMcClennen
Posts: 370
Joined: Sun Mar 09, 2003 9:09 pm
Location: Ontario

Re: Best Glue for Garden Stakes

Postby DonMcClennen » Sat Mar 26, 2016 4:55 pm

GE Silicone 2 will do the job well. I have outside installations now 15yrs old.... outside 4 seasons with NO failures!
"The Glassman"

Valerie Adams
Posts: 587
Joined: Mon Apr 19, 2004 2:49 pm
Location: Santa Rosa, California
Contact:

Re: Best Glue for Garden Stakes

Postby Valerie Adams » Sun Mar 27, 2016 3:13 pm

I'm with Don; silicone is my choice for outdoors.

grammy
Posts: 26
Joined: Fri Nov 17, 2006 10:07 am
Location: Charlotte NC
Contact:

Re: Best Glue for Garden Stakes

Postby grammy » Mon Mar 28, 2016 8:05 pm

Thanks. I did not find the Loctite that was mentioned but got an epoxy for metal to glass.

Peter Angel
Posts: 186
Joined: Fri Oct 31, 2008 9:26 am
Location: Newtown, Sydney, Australia.

Re: Best Glue for Garden Stakes

Postby Peter Angel » Wed Apr 06, 2016 5:31 am

DonMcClennen wrote:GE Silicone 2 will do the job well. I have outside installations now 15yrs old.... outside 4 seasons with NO failures!


Don, do you ever get mold growing on the cured silicone?

Pete
Peter Angel
http://peterangelart.blogspot.com/

A bigger kiln, A bigger kiln, my kingdom for a bigger kiln.

Buttercup
Posts: 561
Joined: Mon Jan 28, 2008 5:22 pm
Location: S.E. Queensland Australia

Re: Best Glue for Garden Stakes

Postby Buttercup » Thu Apr 07, 2016 8:06 pm

Guess you can't replace it with grout, as we now have to do at all the floor/wall junctions in the showers. Damn! Jen


Post Reply

Return to “Techniques and Tools”

Who is online