I was in a hurry to make some discs for garden stakes. So I put a 10" one on a shelf and then decided to put a shelf above it with a 12" disc. Well, there was very ventilation for the bottom glass so I got major devit. Lesson learned. Now to get that stuff off. Since I do not have a sand blaster, I will probably hand grind it. Oh well. :twisted: :twisted: :twisted: :twisted: