grammy
Posts: 26
Joined: Fri Nov 17, 2006 10:07 am
Location: Charlotte NC
Contact:

Devit Spray and Dichoric

Postby grammy » Sat May 14, 2016 9:29 pm

I am making projects that seem to be getting devit on the second firing. These pieces will have dichroic on the top and tack fused. Will the clear coating affect the dichroic? TIA

Marian
Posts: 57
Joined: Mon Dec 06, 2004 5:37 pm
Location: Big Island Hawaii
Contact:

Re: Devit Spray and Dichoric

Postby Marian » Fri May 20, 2016 3:36 am

Yes, it is likely. Better to make a test strip with materials you intend to use. Devit spray can be blotchy or change the color of the dichroic.

Barry Kaiser
Posts: 287
Joined: Mon Jul 25, 2005 6:54 pm
Location: North Carolina
Contact:

Re: Devit Spray and Dichoric

Postby Barry Kaiser » Fri May 20, 2016 8:12 am

There is devit spray, and there is devit spray.
Glass based devit sprays may well cause problems with dichro. I don't use them, so I can't say.
But borax based devit sprays do not affect dichro. Plenty of experience with that.
I have a tutorial on my web site on how to make cheap borax based agent.

Barry

Judd
Posts: 291
Joined: Mon Sep 01, 2003 9:45 am
Location: Arkansas

Re: Devit Spray and Dichoric

Postby Judd » Fri May 20, 2016 12:15 pm

My experience is that Homemade Anti-Devit spray removed iridized surfaces from fusible glass - but I've not tried it on dichroic. Good luck and post pictures please.

grammy
Posts: 26
Joined: Fri Nov 17, 2006 10:07 am
Location: Charlotte NC
Contact:

Re: Devit Spray and Dichoric

Postby grammy » Tue May 24, 2016 11:46 am

Thanks for the reply. I am going to try it later. My art show is over and I am going to relax for a little.


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: No registered users and 36 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com