Page 1 of 1
Devit Spray and Dichoric
Posted: Sat May 14, 2016 9:29 pm
by grammy
I am making projects that seem to be getting devit on the second firing. These pieces will have dichroic on the top and tack fused. Will the clear coating affect the dichroic? TIA
Re: Devit Spray and Dichoric
Posted: Fri May 20, 2016 3:36 am
by Marian
Yes, it is likely. Better to make a test strip with materials you intend to use. Devit spray can be blotchy or change the color of the dichroic.
Re: Devit Spray and Dichoric
Posted: Fri May 20, 2016 8:12 am
by Barry Kaiser
There is devit spray, and there is devit spray.
Glass based devit sprays may well cause problems with dichro. I don't use them, so I can't say.
But borax based devit sprays do not affect dichro. Plenty of experience with that.
I have a tutorial on my web site on how to make cheap borax based agent.
Barry
Re: Devit Spray and Dichoric
Posted: Fri May 20, 2016 12:15 pm
by Judd
My experience is that Homemade Anti-Devit spray removed iridized surfaces from fusible glass - but I've not tried it on dichroic. Good luck and post pictures please.
Re: Devit Spray and Dichoric
Posted: Tue May 24, 2016 11:46 am
by grammy
Thanks for the reply. I am going to try it later. My art show is over and I am going to relax for a little.