Postby jim burchett » Wed Jan 04, 2017 3:46 pm

I have been sawing patternbars on my 10" wetsaw with a Husqvarna Diamond glass blade. Lately the bars 3\8x3\8. Are breaking quite a bit. Have water streams directed to the cut, there is not excessive vibration, blade is dressed frequently. Is it time for a new blade? How do you tell? The bars were well annealed 900 for 2 you then 25 per/hr to 800 75 to 700 then off.Thanks
"No, you cant scare Me, I'm sticking to the UNION. I'm stickin to the UNION till the day I die" Woody Guthrie

The Hobbyist
Posts: 299
Joined: Sun Mar 09, 2003 7:09 pm
Location: Sun City West (NW Phoenix), AZ
Contact:

Re: Diamond Blade

Postby The Hobbyist » Thu Jan 05, 2017 11:11 am

Have you dressed the blade recently?

Jim
"With or without religion, good people can behave well and bad people can do evil; but for good people to do evil—that takes religion. " Steven Weinberg

Valerie Adams
Posts: 587
Joined: Mon Apr 19, 2004 2:49 pm
Location: Santa Rosa, California
Contact:

Re: Diamond Blade

Postby Valerie Adams » Thu Jan 05, 2017 7:31 pm

Are you using a blade stabilizer? That made a big difference on my 10" saw.

jim burchett
Posts: 217
Joined: Sun Jun 29, 2003 4:24 pm
Location: Lenoir, NC

Re: Diamond Blade

Postby jim burchett » Fri Jan 06, 2017 6:02 pm

dress it frequently with a stone from HIS, no stabilizers might try that..read somewhere you can use old 7" blades as stabilizers?
"No, you cant scare Me, I'm sticking to the UNION. I'm stickin to the UNION till the day I die" Woody Guthrie

jim simmons
Posts: 428
Joined: Sun Mar 09, 2003 10:37 pm
Location: Hillsboro Oregon
Contact:

Re: Diamond Blade

Postby jim simmons » Sat Jan 07, 2017 7:55 pm

Stabilizer. Definitely helps.
HIS glassworks.

The other Jim


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: No registered users and 15 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com