I have been sawing patternbars on my 10" wetsaw with a Husqvarna Diamond glass blade. Lately the bars 3\8x3\8. Are breaking quite a bit. Have water streams directed to the cut, there is not excessive vibration, blade is dressed frequently. Is it time for a new blade? How do you tell? The bars were well annealed 900 for 2 you then 25 per/hr to 800 75 to 700 then off.Thanks
Re: Diamond Blade
Posted: Thu Jan 05, 2017 11:11 am
by The Hobbyist
Have you dressed the blade recently?
Jim
Re: Diamond Blade
Posted: Thu Jan 05, 2017 7:31 pm
by Valerie Adams
Are you using a blade stabilizer? That made a big difference on my 10" saw.
Re: Diamond Blade
Posted: Fri Jan 06, 2017 6:02 pm
by jim burchett
dress it frequently with a stone from HIS, no stabilizers might try that..read somewhere you can use old 7" blades as stabilizers?
Re: Diamond Blade
Posted: Sat Jan 07, 2017 7:55 pm
by jim simmons
Stabilizer. Definitely helps.