Postby Steve Immerman » Sun Feb 22, 2004 2:25 pm

I'm trying to figure out a good way to store a gazillion stringers that I pulled in the glory hole. I'm thinking that if I could find some clear plastic tubing, like the "store bought" stringers come in I could make my own holders. So far, I haven't been able to find anything like that. Anybody have any ideas for a source for this? Or a better idea for storage?

Thanks.

Steve

Richard Sinning
Posts: 10
Joined: Tue Jan 27, 2004 9:32 pm

Local Home center

Postby Richard Sinning » Sun Feb 22, 2004 3:10 pm

Head for the home store and pick up some pieces of plastice pvc pipe and caps. Glue the caps on the end and voila, storage for stringers. A little strap hanger and they could be hung anywhere
Richard

Steve Immerman
Posts: 208
Joined: Sun Mar 09, 2003 4:55 pm
Location: Eau Claire, Wisconsin
Contact:

Postby Steve Immerman » Sun Feb 22, 2004 3:13 pm

I had thought of that, but the PVC pipe I have is white. Does it come in a transparent PVC? I was kind of hoping to be able to see the colors.

Steve

Ron Coleman
Posts: 468
Joined: Sun Mar 09, 2003 3:20 pm
Location: Columbus, Ohio USA

Postby Ron Coleman » Sun Feb 22, 2004 3:31 pm

Tubes and Caps aka clear mailing tubes.

http://www.uline.com/Group_74.asp

I've seen longer ones too.

Ron

Rebecca M.
Posts: 126
Joined: Fri Sep 12, 2003 12:15 pm
Location: Myrtle Beach
Contact:

Postby Rebecca M. » Sun Feb 22, 2004 3:43 pm

Here's some more. Maybe a little less expensive. Check out the square tubes 2x24. They're on sale for .99 each. http://www.jcdanczak.com/our_products/cat_7.html

They sell hanging caps too which may be a good storage option.

dee
Posts: 302
Joined: Tue Mar 11, 2003 5:20 pm
Location: Atlanta GA
Contact:

Postby dee » Sun Feb 22, 2004 4:06 pm

Steve Immerman wrote:I had thought of that, but the PVC pipe I have is white. Does it come in a transparent PVC? I was kind of hoping to be able to see the colors.

Steve


steve, being an unreformed packrat, i believe i have a bunch of dichroic frit tubes - would these help? andyes, they are clear and have caps on both ends....
D
Dee Janssen
Unicorn's Creations Studio
http://ucjewelry.com
dee@ucjewelry.com

camaro
Posts: 41
Joined: Mon Mar 10, 2003 2:36 pm
Location: Texas

Stringers

Postby camaro » Sun Feb 22, 2004 6:40 pm

Just a thought, I use clear tubing with plasic chair end caps, you can get the clear tubing various diameters. They work for me.
camaro

Steve Immerman
Posts: 208
Joined: Sun Mar 09, 2003 4:55 pm
Location: Eau Claire, Wisconsin
Contact:

Postby Steve Immerman » Sun Feb 22, 2004 7:19 pm

Dee - I need something at last a couple of feet long. Three feet might be best.

Camaro - do you mean flexible tubing?The shipping tubes might work, I just wish the were longer and narrower....

Steve

Gordon Exon
Posts: 5
Joined: Mon Feb 02, 2004 8:22 pm
Location: Calgary

stringer storage

Postby Gordon Exon » Sun Feb 22, 2004 7:50 pm

the tubes they sell for shop vacuum systems are clear. i don't know about the economics but clearly the source is there

Alecia Helton
Posts: 108
Joined: Mon Aug 25, 2003 12:35 am
Location: outside of Dallas TX

Postby Alecia Helton » Sun Feb 22, 2004 8:16 pm

How about going to a housewares shop and buying storage for spaghetti noddles?

Alecia
Alecia Helton
Wear Original Wonders!
Carrollton TX

Kim Bellis
Posts: 133
Joined: Sat Jun 14, 2003 9:48 pm
Location: Tampa, Florida
Contact:

Postby Kim Bellis » Sun Feb 22, 2004 8:28 pm

Alecia:
I like that idea!!
Kim

Robyn Alexander
Posts: 22
Joined: Fri Jul 04, 2003 7:49 pm
Location: Berkeley CA

Postby Robyn Alexander » Mon Feb 23, 2004 2:27 am

Steve Immerman wrote:Dee - I need something at last a couple of feet long. Three feet might be best.

Camaro - do you mean flexible tubing?The shipping tubes might work, I just wish the were longer and narrower....

Steve


Tap Plastics sells plastic tubes 36" long. You can see them at:
http://www.tapplastics.com/shop/product.php?pid=274&

Nancy Juhasz
Posts: 111
Joined: Sun Mar 09, 2003 10:10 pm
Location: Ohio

Postby Nancy Juhasz » Mon Feb 23, 2004 10:39 am

Steve, Did you ever think of making your own out of plastic or acrylic sheets? This place seems to have the stuff http://www.plaskolite.com/optix-acrylic-sheet.htm
I don't have time right now to do a good search need to be someplace in 20 minutes. Maybe use a broom stick or something as your guide gor size You could buy the caps. Nanc

Bellknap
Posts: 26
Joined: Tue Feb 10, 2004 10:20 am
Location: Columbus, Ohio

PVC pipe display

Postby Bellknap » Mon Feb 23, 2004 5:36 pm

Ok, don't look at the mess around it, but this is how I store my rods for lampworking. I bet you could use the same for your stringers. If you lay them on their side your stringer could hang out a little so you could see what you had easily. I got these at Home Depot and they cut them for me for free. Lydia of OhioImage

charlie
Posts: 961
Joined: Mon Mar 10, 2003 3:08 pm

Postby charlie » Mon Feb 23, 2004 5:40 pm

Steve Immerman wrote:I had thought of that, but the PVC pipe I have is white. Does it come in a transparent PVC? I was kind of hoping to be able to see the colors.

Steve


they make clear pvc, but it's hideously expensive, as compared to white pvc.

Geri Comstock
Posts: 340
Joined: Mon Mar 10, 2003 4:16 pm
Location: Northern CA
Contact:

Postby Geri Comstock » Mon Feb 23, 2004 5:47 pm

Steve -

Maybe a local plastics store might have something you could use. Here in CA we have Tapp Plastics and they have all kinds of strange plastic stuff that anyone could possibly want. I don't know if this is a national chain, though.

Geri

Peg
Posts: 74
Joined: Tue Apr 08, 2003 7:50 am
Location: Bristol, UK

Postby Peg » Wed Feb 25, 2004 8:51 am

I use empty tins than bottles of fine brandy and whisky come in.
Several of them.

Only downside is getting rid of the bottle and contents therein...


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: Google [Bot] and 16 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com