Post by Andrea R »

Hello all it's been a long time !

I have a full sheet of dichroic and can't remember what the best side to cut it on is .

Dichroic up or down ?

Thanks

Andrea
Image
"C'est Moi (Its Me)"
DonMcClennen
Posts: 381
Joined: Sun Mar 09, 2003 9:09 pm
Location: Ontario

Re: cutting dichroic

Post by DonMcClennen »

Score on the back to eliminate damaging dichro coating
"The Glassman"
Andrea R
Posts: 61
Joined: Fri Sep 30, 2005 10:52 am
Location: Canada

Re: cutting dichroic

Post by Andrea R »

Thank Don !!
What I thought but its always good to check and only cut once :)