Tiffany Golden Glass, Carboxylic acid

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
Mustafa Umut Sarac
Posts: 8
Joined: Sun Aug 08, 2010 9:24 pm

Tiffany Golden Glass, Carboxylic acid

Post by Mustafa Umut Sarac »

Any one knows that how tiffany created golden color with carboxylic acid ?

Mustafa Umut Sarac
Istanbul
Joyce Walters
Posts: 80
Joined: Thu Nov 08, 2007 12:06 am
Location: Stevensville MT

Re: Tiffany Golden Glass, Carboxylic acid

Post by Joyce Walters »

I have no knowledge on lusters,
but you might start by reading whatever Corning Glass has to share.
Good luck with your search.
Joyce