Relay Mishap - WarmGlass.com

Relay Mishap

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Tony Smith, Brad Walker

Post Reply
smallbitz
Posts: 154
Joined: Sat Jun 27, 2009 8:44 am
Location: Florida

Relay Mishap

Postby smallbitz » Mon May 07, 2018 6:36 am

I had a large kiln load of (thankfully) first-firing glass that was all double 3mm pieces of 18" x 3" strips. I went to check before bedtime, and three hours after starting the kiln it was already up to 1440°. Other than a few more little champagne bubbles than usual, all look fine this morning. No thermal shock cracks that I can see. After I change the relays, my next step is to do tack fuse on these pieces, then a final slump firing. Should I go ahead with my usual firings OR fire to anneal them before I go any further?

Brad Walker
Site Admin
Posts: 1372
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Relay Mishap

Postby Brad Walker » Mon May 07, 2018 8:26 am

No need to anneal again, just go straight into the next firing. And do change the relays first!

smallbitz
Posts: 154
Joined: Sat Jun 27, 2009 8:44 am
Location: Florida

Re: Relay Mishap

Postby smallbitz » Mon May 07, 2018 10:40 am

Thanks! New relays on the way.


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: No registered users and 75 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com