I am interested in drawing patterns on SLS glass using a cutter, and then inducing devit along the scores themselves. I have worked with intentional devit using laminate technique following much of the late Brian Blanthorn's ideas, but haven't been able to figure this one yet. I have tried a soak at 750ºC, but (surprisingly) the scores were melted and nearly reincorporated into the glass.

Ideas?

Kevin Midgley
Posts: 618
Joined: Mon Mar 10, 2003 11:36 am
Location: Tofino, British Columbia, Canada

Re: Inducing devit along glass scores

Postby Kevin Midgley » Mon May 07, 2018 7:29 pm

SLS glass?
I took notes on Brian Blanthorn's techniques that were on this bulletin board back in 2011.
Don't know if I should repost as other people also posted at that time on the same topic and Brian's are interlaced in the other commentary at that time.
I might also have errors in the saving process due to any editing that I may have done.
I love Brian's work so much I have PSK63
http://www.blanthorn.com/bowls/bowls_1980_1989/portfolio_bowl_86.asp
You can learn by studying actual glass he made.

A lot will depend on your kiln design.


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: Google [Bot] and 23 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com