Page 1 of 1
Inducing devit along glass scores
Posted: Mon May 07, 2018 5:57 pm
by Alexis Dinno
I am interested in drawing patterns on SLS glass using a cutter, and then inducing devit along the scores themselves. I have worked with intentional devit using laminate technique following much of the late Brian Blanthorn's ideas, but haven't been able to figure this one yet. I have tried a soak at 750ÂșC, but (surprisingly) the scores were melted and nearly reincorporated into the glass.
Ideas?
Re: Inducing devit along glass scores
Posted: Mon May 07, 2018 7:29 pm
by Kevin Midgley
SLS glass?
I took notes on Brian Blanthorn's techniques that were on this bulletin board back in 2011.
Don't know if I should repost as other people also posted at that time on the same topic and Brian's are interlaced in the other commentary at that time.
I might also have errors in the saving process due to any editing that I may have done.
I love Brian's work so much I have PSK63
http://www.blanthorn.com/bowls/bowls_19 ... owl_86.asp
You can learn by studying actual glass he made.
A lot will depend on your kiln design.