Postby Laura Mullen » Sun May 20, 2018 3:14 pm

Hi-
I just got a CoreLite shelf for my Skutt1214. Info online about kiln washes for these shelves is mixed. I don’t cast glass, and my highest temp may reach 1470°. I hope to avoid getting any wash stuck to the bottom of my glass, needless to say. Is there a final answer for which wash is preferred for CoreLite shelves?
I’ve had one glass artist tell me he coats his CoreLite shelf once every 6 mos (cleans it at that point, too), and another artist coats the shelf lightly once every firing, cleaning the shelf every 3 mos. any suggestions? I can fire every day for a few weeks, then not at all for months.
Thank you for any insight or cautions you can share with me before I launch into using this shelf!
LauraM

jim simmons
Posts: 412
Joined: Sun Mar 09, 2003 10:37 pm
Location: Hillsboro Oregon
Contact:

Re: Which kiln wash for Core Lite shelves

Postby jim simmons » Sun May 20, 2018 4:11 pm

B.E. kiln wash IMHO
The other Jim

Brad Walker
Site Admin
Posts: 1254
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Which kiln wash for Core Lite shelves

Postby Brad Walker » Sun May 20, 2018 5:27 pm

I just use Bullseye more or less the same as any other shelf. Might need recoating a little more often, but not much difference.

Laura Mullen
Posts: 7
Joined: Mon Sep 19, 2005 10:14 am

Re: Which kiln wash for Core Lite shelves

Postby Laura Mullen » Sun May 27, 2018 11:43 am

Thanks so much for your advice!
LauraM


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: Google [Bot] and 25 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com