Which kiln wash for Core Lite shelves

Posted: Sun May 20, 2018 3:14 pm
by Laura Mullen
Hi-
I just got a CoreLite shelf for my Skutt1214. Info online about kiln washes for these shelves is mixed. I don’t cast glass, and my highest temp may reach 1470°. I hope to avoid getting any wash stuck to the bottom of my glass, needless to say. Is there a final answer for which wash is preferred for CoreLite shelves?
I’ve had one glass artist tell me he coats his CoreLite shelf once every 6 mos (cleans it at that point, too), and another artist coats the shelf lightly once every firing, cleaning the shelf every 3 mos. any suggestions? I can fire every day for a few weeks, then not at all for months.
Thank you for any insight or cautions you can share with me before I launch into using this shelf!

Re: Which kiln wash for Core Lite shelves

Posted: Sun May 20, 2018 4:11 pm
by jim simmons
B.E. kiln wash IMHO
The other Jim

Re: Which kiln wash for Core Lite shelves

Posted: Sun May 20, 2018 5:27 pm
by Brad Walker
I just use Bullseye more or less the same as any other shelf. Might need recoating a little more often, but not much difference.

Re: Which kiln wash for Core Lite shelves

Posted: Sun May 27, 2018 11:43 am
by Laura Mullen
Thanks so much for your advice!