using embedded fused glass in cement countertop
Moderators: Brad Walker, Tony Smith
using embedded fused glass in cement countertop
I am making a kitchenette in our basement - including a cement table top and having professionals fabricate the counters. Has anyone had any experience with using fused glass elements embedded into the concrete -like any inlay (not the recycled glass bits as you see everywhere). Thanks for any advice. Kim
Re: using embedded fused glass in cement countertop
Hi Kim
I have just finished casting and staining a cement table top with a 12 x 12 fused glass textured greenman tile inset into the cement.
I used the reversed process of casting this (table top was on the bottom of the form. The tile appears to be very well set in the cement.
HTH,
Seth
I have just finished casting and staining a cement table top with a 12 x 12 fused glass textured greenman tile inset into the cement.
I used the reversed process of casting this (table top was on the bottom of the form. The tile appears to be very well set in the cement.
HTH,
Seth