Postby raphy » Fri Jul 20, 2018 3:29 pm

mine: for three layer 71/2 x 11 assembled frit sheets. which works

300 1215 2.00
100 1490 :20
9999 910 2:00
100 750 .15
However I am now doing four layers of 12x12 assembled frit sheets. Do you think I need to change this schedule at all. Thank you for any advice, I'm really bad at changing schedules that I know work.

The Hobbyist
Posts: 297
Joined: Sun Mar 09, 2003 7:09 pm
Location: Sun City West (NW Phoenix), AZ
Contact:

Re: firing schedule

Postby The Hobbyist » Sun Jul 22, 2018 10:33 am

I would add/change 50 800 to the anneal for this one and the next.

Jim "The Hobbyist"
"With or without religion, good people can behave well and bad people can do evil; but for good people to do evil—that takes religion. " Steven Weinberg


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: No registered users and 15 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com