Postby anne b » Wed Jun 26, 2019 8:33 am

Wondering if glass laminate (Arco) can be used in fusing. A friend gave me many boxes of this substance (old) in many colors. Can't find anything online about it, except that manufactured laminated glass is used as safety glass. Makes me think it might be something plastic. Very fine powder - like talc. Thanks for any info.
Attachments
IMG_2309.jpg
photo of box

Brad Walker
Site Admin
Posts: 1323
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: fusing glass laminate powder

Postby Brad Walker » Fri Jun 28, 2019 2:23 pm

In general glass laminate is used to laminate two pieces of glass together (like a front windshield in a car). It's a kind of plastic film between the two and can't be fused in the kiln.


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: No registered users and 13 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com