Postby twin vision glass » Mon Jul 15, 2019 10:45 pm

There was a discussion awhile ago about Zircar Luminar MM6 . Many were wanting to know how to use it so I decided to try to help out by working with Zircar and doing a video and some PDF s for them. They have posted the video ( so surprised how older I look :cry: ) but hey it is not about me, it is about an amazing mold material that many do not know how to use it. So hopefully this will help others
https://www.youtube.com/watch?v=le96sNV_b0Y&t=28s

Brad Walker
Site Admin
Posts: 1346
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: MM6

Postby Brad Walker » Tue Jul 16, 2019 8:32 am

Enjoyed the video, can't wait for part 2.

twin vision glass
Posts: 570
Joined: Thu Apr 29, 2004 12:55 am
Location: Invermere,B.C. Canada
Contact:

Re: MM6

Postby twin vision glass » Tue Jul 16, 2019 2:15 pm

Hi dear Brad, hope you are well. A while ago some artists were asking about how to work with Mold Mix 6 so I did this video and Zircar has 4 PDF's also to help others to be able to work with this casting material that has been part of my life for 30 years and I have loved working with it and hope others will now see how great it is.

JestersBaubles
Posts: 689
Joined: Fri Feb 25, 2011 12:01 am
Location: North Logan, UT
Contact:

Re: MM6

Postby JestersBaubles » Fri Jul 19, 2019 11:58 pm

Thank you -- great video!

Dana


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: No registered users and 32 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com