Glues and silicones
Posted: Thu Jul 18, 2019 8:07 am
Interested in recommendations regarding glues and silicones for the following use cases:
1-Assemblage of small, clear glass pieces (e.g. a sculpture composed of different kinds of glasses that aren’t compatible for fusing). I have used Loctite glass glue. It dries clear, stays clear, is fairly strong but I wouldn’t use it for larger pieces. I’ve heard that UV glue is preferable but don’t know what brand.
2-Adhering clear glass permanently to another surface (e.g. glass onto ceramic or vice versa). I’ve used two-part JBWeld clear epoxy, but the company told me it will yellow over time.
3-Repair broken glass. UV glue? If so what kind? I’ve tried Bondix but it did not stay clear. Kevin recommended Lepages 100% glue.
4-Adhere kilncarved transparent glass to another piece of glass for display. Silicone seems logical but I had a heck of a time making a consistent bead.
5-Adhering images printed on paper to glass. I’ve tried acrylic gel medium with mixed results.
6-Adhering glass temporarily to a wall (as in an installation for a month). Silicone can be removed with vinegar (I think), so that seems reasonable. I tried glue dots but they are not strong enough.
7- Securing large glass in a frame (similar to a mirror, as a secondary hold, in addition to staples). CRL silicone was highly recommended by a local glass shop.
8- Bails on glass pendants. I have used E6000 and JBWeld two-part, but at least one of them (maybe both) failed after exposure to heat (sitting in a hot car). I know I should probably ask this in the Jewelry forum but, now that I have your attention...
1-Assemblage of small, clear glass pieces (e.g. a sculpture composed of different kinds of glasses that aren’t compatible for fusing). I have used Loctite glass glue. It dries clear, stays clear, is fairly strong but I wouldn’t use it for larger pieces. I’ve heard that UV glue is preferable but don’t know what brand.
2-Adhering clear glass permanently to another surface (e.g. glass onto ceramic or vice versa). I’ve used two-part JBWeld clear epoxy, but the company told me it will yellow over time.
3-Repair broken glass. UV glue? If so what kind? I’ve tried Bondix but it did not stay clear. Kevin recommended Lepages 100% glue.
4-Adhere kilncarved transparent glass to another piece of glass for display. Silicone seems logical but I had a heck of a time making a consistent bead.
5-Adhering images printed on paper to glass. I’ve tried acrylic gel medium with mixed results.
6-Adhering glass temporarily to a wall (as in an installation for a month). Silicone can be removed with vinegar (I think), so that seems reasonable. I tried glue dots but they are not strong enough.
7- Securing large glass in a frame (similar to a mirror, as a secondary hold, in addition to staples). CRL silicone was highly recommended by a local glass shop.
8- Bails on glass pendants. I have used E6000 and JBWeld two-part, but at least one of them (maybe both) failed after exposure to heat (sitting in a hot car). I know I should probably ask this in the Jewelry forum but, now that I have your attention...