mesh melt turn black - WarmGlass.com

mesh melt turn black

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Tony Smith, Brad Walker

Post Reply
Bonnie Rubinstein
Posts: 171
Joined: Sun May 04, 2003 9:04 pm
Location: River Falls, WI

mesh melt turn black

Postby Bonnie Rubinstein » Wed Aug 14, 2019 3:28 pm

Hi- I am making mesh melts with system 96. Nothing dark, except some small pieces of aventurine green. The rest is firelight white, and light greens and blues, a few blue and green opaques thrown in. For some reason, sections of black result in the melt. It is not spalling- that is small flakes. This is the glass actually turning black, as if there was some incompatibility issue. ( I attached a picture, hope it shows up! ) Thanks for the feedback! Bonnie
Attachments
IMG_2766.jpg
Bonnie Rubinstein

Bonnie Rubinstein
Posts: 171
Joined: Sun May 04, 2003 9:04 pm
Location: River Falls, WI

Re: mesh melt turn black

Postby Bonnie Rubinstein » Wed Aug 14, 2019 3:30 pm

the picture (clearly) was just a before shot of the stack of pre-fired glass.
Bonnie Rubinstein

Brad Walker
Site Admin
Posts: 1372
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: mesh melt turn black

Postby Brad Walker » Thu Aug 15, 2019 8:34 am

Got an after photo?

Bonnie Rubinstein
Posts: 171
Joined: Sun May 04, 2003 9:04 pm
Location: River Falls, WI

Re: mesh melt turn black

Postby Bonnie Rubinstein » Thu Aug 15, 2019 9:09 am

Ha- I broke it up with a hammer to use just the good parts and tossed the black. I will go to studio and see what I can get on a photo.
Bonnie Rubinstein

Bonnie Rubinstein
Posts: 171
Joined: Sun May 04, 2003 9:04 pm
Location: River Falls, WI

Re: mesh melt turn black

Postby Bonnie Rubinstein » Thu Aug 15, 2019 9:56 am

I recall I did take a quick pic prior to the hammer! here it is.
Attachments
IMG_2768.jpg
Bonnie Rubinstein

DonMcClennen
Posts: 372
Joined: Sun Mar 09, 2003 9:09 pm
Location: Ontario

Re: mesh melt turn black

Postby DonMcClennen » Thu Aug 15, 2019 11:27 am

I actually see a lot of darker cathedrals in your pile... they will dominate!!!
"The Glassman"

Bonnie Rubinstein
Posts: 171
Joined: Sun May 04, 2003 9:04 pm
Location: River Falls, WI

Re: mesh melt turn black

Postby Bonnie Rubinstein » Thu Aug 15, 2019 1:37 pm

a couple skinny cobalts and aventurines. So, they turn black? On a mesh melt, are light colors the only options?
Bonnie Rubinstein

Brad Walker
Site Admin
Posts: 1372
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: mesh melt turn black

Postby Brad Walker » Fri Aug 16, 2019 8:26 am

Bonnie Rubinstein wrote: On a mesh melt, are light colors the only options?


I mostly use opaques and clears. Why would light colors be the only option?

Judd
Posts: 291
Joined: Mon Sep 01, 2003 9:45 am
Location: Arkansas

Re: mesh melt turn black

Postby Judd » Fri Aug 16, 2019 12:02 pm

I have had the exact same reaction using the exact same colors. I think the culprit is the transparent yellow. Whenever I do strip construction, or mesh melts, the area where the transparent yellow touches the blue will always darken.

When you stack the glass, place transparent above and below each yellow to minimize the blending, or tell your consumers that you MEANT to do it that way!!! YES! You meant to blend those colors, which explains the PREMIUM price!

Bonnie Rubinstein
Posts: 171
Joined: Sun May 04, 2003 9:04 pm
Location: River Falls, WI

Re: mesh melt turn black

Postby Bonnie Rubinstein » Fri Aug 16, 2019 6:48 pm

hi all,
Thanks for the input.
I just spoke with Oceanside glass. Sent them the pics. This is the synopsis- I was working with reactive colors. Most of the time, at normal firing temps, this is not an issue . But at over 1600 degrees for mesh melts, this is.. the Copper based Blues and the Sulfur based Yellows react to make a deep burgundy and at higher temps, turns black. There you have it! So, they sent me a system 96 reactive chart: http://system96.com/Resources/System96ReactiveChart.pdf
This shows what colors are high to medium reactive, at the higher temps, even the medium reactives can get very dark.

So glad this is solved! Hope this helps others before they run into same situation.

Bonnie
Bonnie Rubinstein


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: No registered users and 40 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com