				Those of you in the know, does this System 96 glass color strike?  If this is the orange I think it is, it color shifts to orange/ brown at fusing temps.
#96-675.5G Godiva
			 
			
					
				Re: Does this Color Strike?
				Posted: Wed Sep 25, 2019 10:00 am
				by Judd
				The pic didn't attach.  Sorry.
Nor did it again.  Well, the color is easily Google-able.  So sorry.
			 
			
					
				Re: Does this Color Strike?
				Posted: Wed Sep 25, 2019 10:53 am
				by Brad Walker
				Probably strikes, most oranges/reds do.