Postby FusedLightStudio » Sun Oct 06, 2019 12:46 pm

I have always used BE “Annealing Thick Slabs” schedules for pieces of any size. The smallest thick pieces I’ve fired have been 6” by 8”.

Another glass artist showed me a smaller piece that was a uniform 1-inch thick, about 4” by 4”, and said it didn’t need to follow the BE schedule for annealing because of the smaller dimensions. Annealed overnight, it was fine five years later. I didn’t have an opportunity to examine it under a polarizer.

Is there a guideline about this? What dimensions are considered a “slab”? How would I determine the annealing schedule for, say, a piece that’s 1” thick and 2” by 2”?
Last edited by FusedLightStudio on Wed Oct 09, 2019 10:58 am, edited 1 time in total.
Lisa Schnellinger
Atlanta, GA

DonMcClennen
Posts: 369
Joined: Sun Mar 09, 2003 9:09 pm
Location: Ontario

Re: Annealing small but thick pieces

Postby DonMcClennen » Mon Oct 07, 2019 4:13 pm

Over many years I have fused numerous smaller thick ( 1",1 1/2", and 2") pieces. Dimensions 2"x 3" , 2 1/2 x 4" and on up to 5" x 20" . I have always used the Bullseye suggested schedule for these based on the smallest dimension of each piece.. My work often sells as corporate awards and I have never had a failure ( probably over 200 pcs. over 20 years) I think if you sell your work then you owe it to your customers to stick with works and the recommendations of the science based Bullseye ramps. If however your just making stuff for yourself it doesn't matter if it fails 2 years down the road when it was left in the sun then experiment away! Just my 2 cents
"The Glassman"


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: No registered users and 46 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com