FusedLightStudio
Posts: 55
Joined: Wed Jan 24, 2018 1:33 pm
Location: Georgia
Contact:

Using oxides as colorants

Postby FusedLightStudio » Thu Nov 14, 2019 8:30 pm

In the studio I inherited from Charlie Holden, I found three bags of powder from the ceramic store: nickel oxide, chromium oxide, and copper carbonate. (The nickel oxide is black, the chromium is a gorgeous dark green, and the copper is a light green.) I know these can be used in ceramic glazing, and I assume they can be used in kilnformed glass, but would like some confirmation and advice.

Can I mix with medium and paint with them? Can I sift them onto the glass like frit powder? What temperature does it need to set?

Thanks in advance for any help.
Lisa Schnellinger
Atlanta, GA

Brad Walker
Site Admin
Posts: 1372
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Using oxides as colorants

Postby Brad Walker » Fri Nov 15, 2019 9:36 am

FusedLightStudio wrote:Can I mix with medium and paint with them? Can I sift them onto the glass like frit powder? What temperature does it need to set?


Either method will work. Full fuse or close to that. Colors may change with different thicknesses.

If sandwiched between glass, there will be some bubbling, which can be attractive (kind of like bubble powder if done correctly).

FusedLightStudio
Posts: 55
Joined: Wed Jan 24, 2018 1:33 pm
Location: Georgia
Contact:

Re: Using oxides as colorants

Postby FusedLightStudio » Fri Nov 15, 2019 5:30 pm

Thank you so much, Brad.

Having recently poked around on some of the Facebook groups for warm glass, I appreciate this forum even more than before (and that was already a lot).
Lisa Schnellinger
Atlanta, GA

Michael Stevens
Posts: 73
Joined: Thu Dec 26, 2019 2:52 pm

Re: Using oxides as colorants

Postby Michael Stevens » Fri Jan 03, 2020 6:40 pm

how could make the painting medium?

Brad Walker
Site Admin
Posts: 1372
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Using oxides as colorants

Postby Brad Walker » Fri Jan 03, 2020 9:29 pm

Michael Stevens wrote:how could make the painting medium?


You can use anything that will mix with the oxides and that burns off cleanly in the kiln. Many glues will work or if you can get some ethyl methyl cellulose or carboxy methyl cellulose (CMC) you can make your own glue that will work well.

Michael Stevens
Posts: 73
Joined: Thu Dec 26, 2019 2:52 pm

Re: Using oxides as colorants

Postby Michael Stevens » Sat Jan 04, 2020 8:50 am

I used Aloe gel for glass pigments worked ok.


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: No registered users and 39 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com

cron