Postby jim burchett » Wed Nov 20, 2019 11:35 am

I am trying to find a reliable adhesive to secure an approx6×6 double thickness of glass to a small piece of flattened bronze rod approx 1/4"x1/2" securely. I have tried E6000 , gorilla glue epoxy, and Hxtal. A 5 day set up for the Hxtal is a bit cumbersome, and properly mixing very small quantities is an adventure. They all work, sort of. Any suggestions appreciated. These are used to support the glass at an angle above a platform. Thank.
"No, you cant scare Me, I'm sticking to the UNION. I'm stickin to the UNION till the day I die" Woody Guthrie

Bert Weiss
Posts: 2338
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Re: Adhesive Question

Postby Bert Weiss » Sun Jan 05, 2020 4:46 pm

Try Hang Your Glass. Used properly it should provide a bond stronger than the glass.

Or trying heating the Hyxtal a bit to make it set up quicker.
Bert

Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions

Dick
Posts: 80
Joined: Sun May 01, 2005 9:34 pm
Location: San Diego
Contact:

Re: Adhesive Question

Postby Dick » Sun Jan 05, 2020 7:56 pm

Better off with Loctite Hysol E-30cl. Uses a gun with mixing tube, so no guessing or mess. Made specifically to work with glass and metal. I have hung 21" round pieces 3/4" thick with just a dime size spot of glue on my hanger. 24 hour cure. All others mentioned I have tried and eventually had problems with. This is crystal clear non yellowing. You can get it online, ebay etc.

Kevin Midgley
Posts: 713
Joined: Mon Mar 10, 2003 11:36 am
Location: Tofino, British Columbia, Canada

Re: Adhesive Question

Postby Kevin Midgley » Mon Jan 06, 2020 11:58 am

No, Dick that resin has a 7 day full cure.

Brad Walker
Site Admin
Posts: 1372
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Adhesive Question

Postby Brad Walker » Mon Jan 06, 2020 9:42 pm

Kevin Midgley wrote:No, Dick that resin has a 7 day full cure.


You sure? Grainger says 24 hours: https://www.grainger.com/product/LOCTITE-E-30CL-2VRH9

Kevin Midgley
Posts: 713
Joined: Mon Mar 10, 2003 11:36 am
Location: Tofino, British Columbia, Canada

Re: Adhesive Question

Postby Kevin Midgley » Tue Jan 07, 2020 6:18 pm

If it takes a week for full chemical resistance then it is still curing to maximum strength. The week came from looking it up online on the company website.
For sure, heat curing speeds up strength gain in most epoxies.
It looks to be similar in strength to glue I use so I'll stick with what I know.
I do know that those squeeze the plunger and squirt out two bands of glue types are for me notoriously difficult to get evenly controlled amounts dispensed.
I've gone so far as to cut them separate.
Of interest, it has been suggested by one company to store the partially used glue dispenser 'nozzle up' to aid in evenivity.

Tony Smith
Posts: 1037
Joined: Sun Mar 09, 2003 5:59 pm
Location: Massachusetts, USA
Contact:

Re: Adhesive Question

Postby Tony Smith » Wed Jan 08, 2020 11:05 pm

Dick is correct.
Full strength cure is 24 hrs at room temp. Max chemical resistance takes a full week.

Tony
The tightrope between being strange and being creative is too narrow to walk without occasionally landing on both sides..." Scott Berkun

Dick
Posts: 80
Joined: Sun May 01, 2005 9:34 pm
Location: San Diego
Contact:

Re: Adhesive Question

Postby Dick » Sun Jan 12, 2020 6:51 pm

Thanks guys. Got the info straight from a rep who demoed at our glass assoc. I use it all the time


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: Google [Bot] and 53 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com