copper inclusion

Postby Michael Stevens » Sat Jan 11, 2020 10:26 pm

I wanted to add this thin copper 2mm thick twisted copper. into a 5inch diameter glass orb. would the metal cause breakage because too thick. leaf or foil wouldn't give the effect I was looking for.

is there a formula for dimension of metal inclusion vs thickness of glass object?

Brad Walker
Site Admin
Posts: 1372
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: copper inclusion

Postby Brad Walker » Sun Jan 12, 2020 12:14 am

2mm is too thick. It will almost certainly crack.

No formula that I'm aware of. It would depend on the particular metal, of course.

Michael Stevens
Posts: 73
Joined: Thu Dec 26, 2019 2:52 pm

Re: copper inclusion

Postby Michael Stevens » Mon Jan 13, 2020 8:43 am

I'm. sorry I meant .2mm

Brad Walker
Site Admin
Posts: 1372
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: copper inclusion

Postby Brad Walker » Mon Jan 13, 2020 8:59 am

Michael Stevens wrote:I'm. sorry I meant .2mm


.2mm should be thin enough. Try a small piece as a test.


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: Google [Bot] and 47 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com