Postby Dick » Thu Jan 30, 2020 6:08 pm

So, I just bought a used bell kiln, and it arrived damaged. i have decided to rebuild the top with all new fiber board, blanket and elements. Would like to know what elements you guys would recommend, and top only or top and side?

Firing chamber 48x48x18"
240 volt single phase


Want to be able to go to 1850. Not often, but want the capability.

Thanks

Dick

Brad Walker
Site Admin
Posts: 1372
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: bell kiln repair

Postby Brad Walker » Fri Jan 31, 2020 8:28 am

For fiber, top only should work.

For brick, both.

Kevin Midgley
Posts: 713
Joined: Mon Mar 10, 2003 11:36 am
Location: Tofino, British Columbia, Canada

Re: bell kiln repair

Postby Kevin Midgley » Fri Jan 31, 2020 1:07 pm

Kanthal A1


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: No registered users and 57 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com