Float Glass

Postby Goldfinger » Tue Feb 24, 2004 12:47 pm

As someone who new to the board and glass fusing in general. the term
"float glass" keeps popping up. I went to the archives to try and find out what it is- to no avail. Can somebody give me a definition?

Thanks

Steve

Bert Weiss
Posts: 2337
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Re: Float Glass

Postby Bert Weiss » Tue Feb 24, 2004 1:27 pm

Steve Eshbaugh wrote:As someone who new to the board and glass fusing in general. the term
"float glass" keeps popping up. I went to the archives to try and find out what it is- to no avail. Can somebody give me a definition?

Thanks

Steve

Steve

It is the flat smooth stuff they put in windows. In the archives are various links to sites that explain how the glass is floated on molten tin. It comes in thicknesses from very thin to 1" thick and in various tints. They make a lot of it worldwide so it is accessible and inexpensive, although not always compatible. It is always compatible with itself though.
Bert

Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions

Paul Tarlow
Posts: 344
Joined: Sun Mar 09, 2003 4:06 pm
Location: Helios Kiln Glass Studio - Austin
Contact:

Postby Paul Tarlow » Tue Feb 24, 2004 1:42 pm

Today I picked up some 3/8 float.

Any tips on getting the score to run?

The torch is waiting :)

Btw, the UV light arrived yesterday. I was happily suprised to see just how obvious it is to detect the tin side.

- Paul

Goldfinger
Posts: 54
Joined: Wed Jan 07, 2004 11:07 am
Location: Missouri

Float Glass

Postby Goldfinger » Tue Feb 24, 2004 1:52 pm

Bert: I did start going through the archives but it probably would have taken two weeks to find the links. There are so many threads.

I take it "float glass " is simply a generic term. It could apply to any glass made by the "float" process initially.

Steve

Bert Weiss
Posts: 2337
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Postby Bert Weiss » Tue Feb 24, 2004 3:35 pm

Paul Tarlow wrote:Today I picked up some 3/8 float.

Any tips on getting the score to run?

The torch is waiting :)

Btw, the UV light arrived yesterday. I was happily suprised to see just how obvious it is to detect the tin side.

- Paul


Paul

You may have to explain better what you want to cut. First of all make sure that you are using a cutter with a 134º angle wheel. Ther Toyo Tap Wheel custom grip is my cutter of choice. Second be sure to use kerosene. Paint the glass with the kero before you score. Press hard enough to make your cutter sing. There is a too hard and a too soft pressure.

For a circle, leave plenty of extra room around the circle. 2" all around is minimum for me. I make a tool with a cheap slotted screw driver. Heat it up red hot and let it cool in the air. Then grind it with a slight rocker (convex). Now you have a tapping tool. after you make the score, flip the glass over and place your tool directly over the score on a place that has plenty of extra glass and is not the spot where you began and ended the score. hit it with the hammer just hard enough to begin the run. Now place the tool at the edge of the run or just beyond there and hit again. Now follow around until the run goes around 360º. Now use the torch to complete the run through the thickness of the glass.

For a straight cut you can simply put a peg directly under the end of your score and push on both sides of the glass. If scored right, it will run straight to the end. I like the Toyo Heavy glass pliers from CRL as my tool of choice for running a score. The only catch is that you have to buy a cutter you don't need as they only come in a kit.
Bert



Bert Weiss Art Glass*

http://www.customartglass.com

Furniture Lighting Sculpture Tableware

Architectural Commissions


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: No registered users and 59 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com