Michael Stevens
Posts: 51
Joined: Thu Dec 26, 2019 2:52 pm

transparent glass turns opaque

Postby Michael Stevens » Sun Apr 05, 2020 8:17 pm

I fused some red glass and it was fine, but I. used similar glass and did a lot melt at higher than fusing temps and it turned opaque, the other colors were fine, I thought maybe debit but it's happened 2 times same color.

does this happen to anyone

Brad Walker
Site Admin
Posts: 1323
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: transparent glass turns opaque

Postby Brad Walker » Sun Apr 05, 2020 9:24 pm

Very common, especial with reds. The higher the temperature, the more likely.


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: No registered users and 16 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com