I fused some red glass and it was fine, but I. used similar glass and did a lot melt at higher than fusing temps and it turned opaque, the other colors were fine, I thought maybe debit but it's happened 2 times same color.

does this happen to anyone

Re: transparent glass turns opaque

Posted: Sun Apr 05, 2020 9:24 pm
by Brad Walker
Very common, especial with reds. The higher the temperature, the more likely.