Postby Michael Stevens » Tue Apr 07, 2020 8:37 pm

I made some molds from shells as casted them, they have nice texture if I tack fuse to a project will the texture be flattened. Or is the only solution to glue. them on?

I guess I could use powdered glass and paint the details to look like the pattern. but I was hoping to. keep the original pattern, my daughter collected. these shells so I wanted a special piece.

Brad Walker
Site Admin
Posts: 1323
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: keeping Texture on glass

Postby Brad Walker » Wed Apr 08, 2020 8:01 am

If you tack fuse at a low enough temperature you'll keep most of the texture. 1350F/730C is high enough to stick glass together and retain most of the texture. The higher above that you go, the more texture you will lose.

Barry Kaiser
Posts: 268
Joined: Mon Jul 25, 2005 6:54 pm
Location: North Carolina
Contact:

Re: keeping Texture on glass

Postby Barry Kaiser » Wed Apr 08, 2020 12:04 pm

Use a low temperature flux, or a glass paint as a glue. I've done a lot of these.


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: Google [Bot] and 21 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com