Soft fuse with flow?
Moderators: Brad Walker, Tony Smith
-
Mark Wright
- Posts: 49
- Joined: Mon Dec 13, 2010 12:43 pm
- Location: Raleigh, NC
Soft fuse with flow?
Looking for help on how to achieve the texture in this picture from Pinterest. So far, I have not been able to reproduce it.
-
Michael Stevens
- Posts: 83
- Joined: Thu Dec 26, 2019 2:52 pm
Re: Soft fuse with flow?
Contour fuse should do it. maybe. somewhere between tack fuse and contour fuse temps. the trick is to layer the glass long to short. I use a SS cake pan to. hold the shape while I'm forming.
-
Mark Wright
- Posts: 49
- Joined: Mon Dec 13, 2010 12:43 pm
- Location: Raleigh, NC
Re: Soft fuse with flow?
Thanks for the hints. Based on your comment of using a cake pan it appears it also needs to be dammed. I'll give it a try.
-
Michael Stevens
- Posts: 83
- Joined: Thu Dec 26, 2019 2:52 pm
Re: Soft fuse with flow?
I use the cake pan to create the shape, don't need to cook it in that pan if you want organic and varied length. but I prefer even edge, I line the pan with kiln paper
Re: Soft fuse with flow?
are those edges of strips or stringers?
Re: Soft fuse with flow?
Don- it's strips on edge, cut in different widths so some will flop and flow. Watching the kiln is crucial until you know what happens when- you want the stuff stuck firmly to itself and the edges rounded nicely.