Ceramaguard for carving?

Postby DeniseNM » Thu Sep 17, 2020 1:36 pm

Hi!

I just bought some of the ceramaguard. I am wanting to make small casting shapes in it (small hearts, flowers, etc.). Am I right in thinking I can carve into the smooth side with some sort of tool? And then kiln wash before firing? Or Zyp? Any suggestions on tools to use to carve? Any other suggestions on uses?

Brad Walker
Site Admin
Posts: 1363
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Ceramaguard for carving?

Postby Brad Walker » Thu Sep 17, 2020 2:14 pm

I use it for carving all the time. You can carve it with any tool that will carve wood or a linoleum block. I carve more intricate designs with a CNC machine.

After carving, you can kiln wash or use a sheet of thinfire over the Ceramaguard. The thinfire will hold together fine for the firing and will give you more detail than kiln wash.

Don't carve on the painted side, the paint flakes off after the first firing or so. You can sand the unpainted side if you wish.


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: No registered users and 60 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com