Postby LCS » Sun Nov 22, 2020 2:26 pm

How long do I have to wait after a full fused piece can be draped?

Brad Walker
Site Admin
Posts: 1363
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Wait time

Postby Brad Walker » Sun Nov 22, 2020 3:39 pm

Do you mean how long after it cools to room temperature or something else?

LCS
Posts: 6
Joined: Mon Aug 20, 2007 9:44 am

Re: Wait time

Postby LCS » Sun Nov 22, 2020 4:53 pm

Yes ... after it cools to room temperature.

Brad Walker
Site Admin
Posts: 1363
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Wait time

Postby Brad Walker » Sun Nov 22, 2020 5:45 pm

If you wait until it cools, you can slump or drape immediately if you wish.

LCS
Posts: 6
Joined: Mon Aug 20, 2007 9:44 am

Re: Wait time

Postby LCS » Sun Nov 22, 2020 6:21 pm

THANK YOU!


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: No registered users and 26 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com