crisp lines with powders and frit

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
jim simmons
Posts: 478
Joined: Sun Mar 09, 2003 10:37 pm
Location: Hillsboro Oregon
Contact:

crisp lines with powders and frit

Post by jim simmons »

20201108_131705_001_resized_3.jpg
I would like[fimg=][/fimg] to know how to create nice crisp lines between different colored powders and fine frit
like this pic
The other Jim
Michael Stevens
Posts: 83
Joined: Thu Dec 26, 2019 2:52 pm

Re: crisp lines with powders and frit

Post by Michael Stevens »

when I sift or brush on powders and frit, I create barriers using bendable plastic ruler. stencils or brush.

or could use a stringer bent to shape then glued down if you want border line. and fill in. like cloisone style
JestersBaubles
Posts: 705
Joined: Fri Feb 25, 2011 12:01 am
Location: North Logan, UT
Contact:

Re: crisp lines with powders and frit

Post by JestersBaubles »

You could use Liquid Glassline and then fill in with frit. Google it - Richard La Londe. Basically CMC & glass powder, piped through a cake decorating bag. There's a free tutorial out on the internet somewhere.